| Sign In | Join Free | My futurenowinc.com |
|
Brand Name : ABOOM
Model Number : Incoloy A-286
Certification : EN 10204 Type 3.1
Place of Origin : CHINA
MOQ : 1000kgs
Price : USD Negotiable
Payment Terms : T/T
Supply Ability : 200 TONS PER MONTH
Delivery Time : 7-15dyas
Packaging Details : Standard export packaging
TYPE OF MATERIAL : Ni-base alloy steel
PRODUCT : Incoloy A-286 Fe-25Ni-15Cr-based superalloy sheet
STANDARD : ASTM B409
GRADE : Incoloy A-286 / NS66286 / ZbNCT25 / P.Q.A286
Manufacturing process : The steel melt shall be refined with AOD or equivalent.
Heat Treatment : shall be supplied in the solution annealed/water quenched condition.
Surface Finish : Descaled, White Pickled, and Passivated Condition
testing facility : Accept third party testing such as SGS
NS66286 / ZbNCT25 Incoloy A 286 Fe 25Ni 15Cr Based Superalloy Sheet Stock
Incoloy A-286 Fe-25Ni-15Cr-based superalloy sheet stock NS66286 / ZbNCT25
Material grade: Incoloy A-286 nickel-based alloy
US grade: UNS NS66286
French grade: ZbNCT25
Incoloy A-286 nickel-based alloy sheet:
Incoloy A-286 nickel-based alloy is Fe-25Ni-15Cr-based high temperature alloy, which is comprehensively strengthened by adding molybdenum, titanium, aluminum, vanadium and trace boron. Below 650 ℃, it has high yield strength, long-lasting, creep strength, and has good processing plasticity and satisfactory welding performance. It is suitable for manufacturing high-temperature bearing parts of aero-engines, such as turbine discs, press discs, rotor blades, and fasteners, which work under 650 ℃ for a long time.
Chemical composition of Incoloy A-286 (NS66286) nickel-based alloy: see Table-1:
Table-1 %
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.08 | 1.00 | 1.00-2.00 | 0.030 | 0.020 | 13.5-16.0 | 24.0-27.0 | 1.0-1.5 | - |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | V≤ | W≤ | B≤ |
| - | 0.04 | 1.75-2.30 | Balance | - | - | - | 0.001-0.01 |
Note:
1. The standard for cold drawn rods, round cakes and ring blanks stipulates ω (Ti) of 1.80% to 2.35%.
2. The standards for hot-rolled and cold-rolled sheets stipulate that ω (B) is 0.003% to 0.010%, ω (Mn) ≤2.00%, ω (P) ≤0.020%, and ω (S) ≤0.015%.
3. Cold drawn wire standards stipulate that ω (Al) ≤ 0.35%, ω (Ti) 1.75% to 2.35%, ω (Si) 0.40% to 1.00%, ω (P) ≤ 0.020%, and ω (S) ≤ 0.015. %.
4. The standards for cold heading wire materials stipulate ω (Ti) 1.75% to 2.35%, ω (Si) 0.40% to 1.00%, ω (P) ≤ 0.025%, and ω (S) ≤ 0.020%.
5. The standard for hot-rolled and forged bars requires ω (Cu) ≤ 0.25%.

|
|
NS66286 / ZbNCT25 Incoloy A 286 Fe 25Ni 15Cr Based Superalloy Sheet Stock Images |